3D printing tolerances are decided on the drawing, not on the printer's datasheet. When a design office hands over an FDM or SLA part, the same question always comes up: what tolerance can you write down without asking for the impossible, or paying for inspection that serves no purpose? The answer depends on the technology, the material, the part's orientation and its finish. Below: the basic notions, the orders of magnitude published by manufacturers, what makes the actual dimension vary, how to dimension a printed part, and how to validate it all on a test part.

Accuracy, precision, tolerance: three different notions

Datasheets often mix these three words up. Formlabs' guide to 3D printing accuracy and precision separates them as follows:

  • Accuracy: the gap between the measured part and the CAD dimension.
  • Precision (repeatability): how consistent the measurements are from one part to the next.
  • Tolerance: the permitted deviation, set by the designer according to what the part must do. It is not a property of the printer.

The first two are judged separately: a part can come out with the same deviation every time, or vary around the right dimension. Formlabs also points out that holding a tighter tolerance costs more, in manufacturing as well as in quality assurance. So you only tighten it where the function requires it.

3D printing tolerances: what manufacturers publish for FDM and SLA

Here are the typical values published by two players in the industry for their own machines and processes. They are orders of magnitude, not guarantees, and not Osmoz 3D values.

ProcessPublished valueSource
SLA/DLP, features 1 to 30 mm±0.15% (lower limit ±0.02 mm)Formlabs
SLA/DLP, features 31 to 80 mm±0.2%Formlabs
SLA/DLP, features 81 to 150 mm±0.3%Formlabs
FDM±0.5% (lower limit ±0.5 mm)Formlabs
FDM "prototyping"±0.5% (lower limit ±0.5 mm)Protolabs
FDM "industrial"±0.3% (lower limit ±0.3 mm)Protolabs

These values are expressed as a percentage of the dimension, with a floor. On a small dimension the lower limit applies; on a large one, the permitted deviation grows with size. For example, ±0.5% with a ±0.5 mm floor means ±0.5 mm for any dimension up to 100 mm, after which the published deviation increases.

The two Protolabs rows correspond to Protolabs' two FDM offerings ("prototyping" and "industrial"), described on its FDM page. They describe Protolabs' service, not that of another workshop, and not ours. For SLS, Formlabs publishes ±0.5% or 0.3 mm, whichever is larger. At Osmoz 3D, FDM and SLA are done in-house and SLS is subcontracted. For a refresher on how each process works, see FDM, SLA or SLS: understanding 3D printing technologies.

What makes the actual dimension vary

The same printer does not hold the same tolerance on every dimension of a part. 3D printing accuracy depends on the technology, but also on orientation, geometry, material and finish.

Orientation and geometry

  • The part is built layer by layer. It does not behave the same way in the plane of the layers and along the height (Z axis): a vertical dimension is not treated like a horizontal one.
  • On sloped or curved surfaces, the stacked layers form steps (the staircase effect). The measured value then depends on where you place the instrument.
  • Holes and bores often come out smaller than drawn, especially when their axis is horizontal. Their dimension is checked on the test part.
  • Large flat areas and thin walls can distort. Overhangs printed on supports keep marks once those supports are removed.

For two surfaces that slide against each other, Formlabs measured lower friction when the layers of the two parts were oriented perpendicular to each other. In practice: the print orientation is decided together with the dimensioning, not afterwards.

Material and post-processing

  • FDM: the part shrinks and can warp as it cools. Formlabs notes that ABS is more prone to this than PLA, because it shrinks more.
  • SLA: post-curing makes the resin shrink. The manufacturer's software compensates for this shrinkage (PreForm, in Formlabs' case), but the effect still needs checking on a real part.
  • Finishing: sanding an FDM part to remove support marks and layer lines changes its dimensions slightly. The drawing should state which surfaces stay as printed.

Material choice therefore also depends on the dimensions you need to hold. The criteria are covered in choosing the right material for your project.

How to dimension the drawing of a printed part

A drawing designed for machining, with a tight tolerance on every dimension, does not carry over well to a printed part. Dimensioning a printed part rests on a simple distinction: the few dimensions that matter, and all the others.

Tolerance only the functional dimensions

Functional dimensions are the ones that ensure assembly, sealing, guiding or the interface with another part. There are few of them, and each carries an explicit tolerance on the drawing. Also show the datum surfaces, the ones those dimensions are measured from: they are what inspection will rely on. All other dimensions stay free and fall under the general tolerance.

Agree on a general tolerance

For untoleranced dimensions, the title block refers to a general tolerance. The usual reference is ISO 2768-1 (General tolerances — Part 1: Tolerances for linear and angular dimensions without individual tolerance indications). This standard was designed for machining and sheet metal work: applying it as is to a printed part is a choice to agree with the manufacturer, not a guarantee. Another option is to write a general tolerance value directly, decided with the printer after the test part.

Assemblies: think in functional clearance

Shaft and bore, clips, slides, inserts: these assemblies are designed with functional clearance, free, sliding or light interference, depending on what the part has to do. The clearance is drawn into the model, then adjusted after the test. If a standardised fit to ISO 286 (Geometrical product specifications (GPS) — ISO code system for tolerances on linear sizes) is required, state it explicitly on the drawing and validate it on a test part. Redesigning the part for printing also helps: see adapting a technical part for 3D printing.

What the drawing should state beyond geometry

  • the preferred print orientation, or the surfaces to favour;
  • the datum surfaces and the functional surfaces;
  • the intended material and the use (temperature, load, contact);
  • the surfaces to leave as printed and those to finish;
  • the dimensions to inspect, and how to measure them.

This information is prepared before sending the file. The full process is described in preparing your 3D print.

Validate on a test part before freezing the drawing

The tolerance actually held is measured on a part, not on a datasheet. Formlabs says so itself: the best way to evaluate a printer is to inspect real parts and, for assemblies, to print test models in several materials. For a given part, the checklist is as follows:

  • print the test part in the material, technology and orientation planned for the run;
  • apply the same post-processing as on the final part;
  • include the functional dimensions and assembly features (hole and shaft, clearances, clips), possibly on a test coupon reduced to those areas;
  • print several copies, to judge repeatability and not just accuracy;
  • measure the drawing's dimensions, noting the instrument used and the datum surfaces;
  • assemble the part with its mating part, in real conditions;
  • record the deviations, correct the model or the drawing (clearances, compensation), then run another test if needed;
  • freeze the drawing only after validation: it becomes the reference for the small production run.

To go further, ISO/ASTM 52902 (Additive manufacturing — Test artefacts — Geometric capability assessment of additive manufacturing systems) describes test geometries and the measurements to take on them. It is a useful reference, not a required step to validate a part. Validation points are set from the start, as explained in the technical project study.

In short

  • Few toleranced dimensions: only the functional ones, with their datum surfaces.
  • A general tolerance agreed with the printer, ISO 2768-1 or a direct value.
  • Clearances designed for printing, and any standardised fit stated on the drawing.
  • A test part, under production-run conditions, before freezing the drawing.

Got a drawing to print?

Send us your dimensioned drawing and your 3D model, with the critical dimensions marked. We discuss it before printing: orientation, material, test part. If we design or modify the model for you, also read what you need to know about the handover of design files.

Going further: discover our technical project study.